fig13

Recent progress of sulfide electrolytes for all-solid-state lithium batteries

Figure 13. (A) Interface configuration for Li/Li6PS5Cl (top) and Li/N-doped Li6PS5Cl (below) after structure relaxation by DFT calculations. (B) Critical current densities of Li6+xPS5-xNxCl electrolytes as a function of N content x. Reproduced with permission[60] (Copyright 2021, Royal Society of Chemistry). Galvanostatic symmetric cell, Li | SE | Li voltage profiles at 50 °C. (C) and (D) Li plating and stripping performance of Li6PS5Cl and Li6.3P0.9Cu0.1S4.9Cl1.1 at 3 mA cm-2, respectively. Reproduced with permission[133] (Copyright 2021, Elsevier).